Shijiazhuang Zhongqian Pump Industry Co., Ltd. · Slurry pumps / Spare parts / Technical support
ZQZhongqian PumpZHONGQIAN PUMP
Home/Slurry Pump Wetted Part Materials
MATERIALS

Slurry Pump Wetted Part MaterialsA05, Cr26, A49, Cr30A and rubber — chosen by duty

Changing the grade on the same pump can multiply wear life. The decision rests on particle size and shape, pH and chloride, and slurry temperature — not on hardness alone.

We supply wetted parts in two families: high-chrome iron, split into A05, A49 and Cr30A by corrosion requirement, and rubber lining for fine-particle corrosive duty. The table below sets out hardness, corrosion limits and typical applications.

High chrome slurry pump throatbush
Slurry Pump Wetted Part Materials
THREE CRITERIA

Read the slurry first, the price list second

Hardness answers abrasion only. Corrosion and temperature are solved by the matrix and the alloying elements, not by raising HRC.

GRADE COMPARISON

Grades we supply and where they belong

Hardness figures are published values. Entries marked "per test certificate" have no public figure and are not estimated here.

GradeTypeHardnessCorrosion resistanceTypical use
A05 (KmTBCr26)High-chrome white ironHRC 58–62Alkaline slurry; not for strong acidsImpellers, volute liners, throatbushes and frame plate liners
A49High-chrome alloy, austenitic matrix + carbidesHRC 44–50pH 4 sulphuric acid, pH 13 sodium hydroxide, moderate chlorideFGD slurry pump impellers and liners
Cr30AHigh-chrome iron, higher carbide contentPer test certificateWear-driven; confirm corrosion case by caseFGD pump impellers and wear plates
2605NCorrosion-resistant alloy ironPer test certificateGypsum slurryFGD pump casings and back cover plates
GLH-5Same family as 2605NPer test certificateCorrosion-drivenFGD casings and back cover plates, interchangeable with 2605N
Natural rubberElastomer lining over a steel corePer compound (Shore A)Dilute acids and alkalis, fine-particle slurry; not for oils or strong oxidisersImpellers, liners and throatbushes in fine-particle corrosive duty
BEYOND HARDNESS

Hardness is not the only number that matters

Treating HRC as the sole criterion is the most common selection error.

BY DUTY

Four typical duties and what we recommend

These are starting points; the slurry analysis and the wear pattern of the failed part take precedence.

DutyRecommendedReason
Coarse, angular, high concentration (tailings, mill discharge)A05 / Cr26 high-chromeBalances hardness with resistance to chipping; thick sections wear to limit
Fine particles, mild corrosion, alkaline pH (concentrate, coal slurry)Rubber lining or A05Rubber resists fine-particle cutting, is light and fast to change
Wet FGD gypsum slurry (pH 4–7, high chloride, ≤65 °C)A49 wetted parts + 2605N / GLH-5 casingAustenitic matrix resists acid and chloride; carbides resist gypsum wear
Alumina, chlor-alkali and similar corrosive abrasive dutyCorrosion grade plus dual mechanical sealCorrosion dominates; seal and material upgrade together
REPLACEMENT

When to replace: wall thickness, not months in service

The same part can last several times longer in a different duty. Calendar-based replacement is neither economical nor safe.

FAQ

Slurry Pump Wetted Part Materials — frequently asked questions

Are A05 and Cr26 the same material?

A05 is the trade grade; KmTBCr26 is the standard designation for high-chrome abrasion-resistant white iron. They describe the same family. Order against the drawing and the mill certificate, since composition and hardness vary by heat.

Does higher hardness always mean longer wear life?

For fine-particle abrasion, broadly yes. For coarse impact duty, excessive hardness brings chipping risk. In corrosive duty hardness barely matters — the matrix decides.

Why use A49 instead of A05 in FGD pumps?

FGD gypsum slurry typically runs at pH 4–7 with high chloride. A05 matrix corrodes, then carbides spall. A49 is softer but its austenitic matrix resists the acid and chloride, giving longer overall life.

Can rubber parts run in coarse particle duty?

No. Sharp coarse particles cut and tear the lining; once it separates from the steel core the part fails quickly. Use high-chrome metal for that duty.

Can we change the material without changing the pump model?

Usually yes. Metal and rubber builds are interchangeable on some sizes, but the mating dimensions and fasteners must be checked — it is not a drop-in swap on every size.

Next step

Send the duty and we will name the grade

We need the slurry, the particle size and shape, weight concentration, pH, chloride content, temperature, and the pump model or a photo of the worn part. With those we can confirm the grade and the part number in one reply.

Send an inquiry

We reply within one business day. You can also call +86 188 0321 2220.

Your details are used for this inquiry only.

Model and spare part identification

Please provide the pump model, nameplate data and duty parameters by phone or email. Performance charts and manuals can be read online.

Click outside or press Esc to close